The hydration phase and pore structure formation in the blends of sulfoaluminate-belite cement with Portland cement

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

2
27
0

Year Published

2005
2005
2016
2016

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 70 publications
(29 citation statements)
references
References 15 publications
2
27
0
Order By: Relevance
“…These findings are similar to those of MDF materials [62,63]. • Region III (over 550°C): this temperature region is characteristic for CaCO 3 decomposition [62][63][64][65][66][67][68][69].…”
Section: Thermal Properties Of C-s-h Pva and C-s-hpn Materialssupporting
confidence: 77%
“…These findings are similar to those of MDF materials [62,63]. • Region III (over 550°C): this temperature region is characteristic for CaCO 3 decomposition [62][63][64][65][66][67][68][69].…”
Section: Thermal Properties Of C-s-h Pva and C-s-hpn Materialssupporting
confidence: 77%
“…iii) Region III (over 550 °C): this temperature region is characteristic for structural water and CaCO 3 decomposition [69][70][71][72][73][74][75][76]. Since the amount of structural water and CaCO 3 (which may formed during the synthesis of C-S-H and C-S-HPN materials) is very low, DTG peaks corresponding to the release of H 2 O, and CO 2 from CaCO 3 are very weak or insignificant.…”
Section: Tg and Dtg Studies Of C-s-h Paa And C-s-hpn Materialsmentioning
confidence: 99%
“…• RT-250°C: this is the region of C-S-H decomposition [36][37][38][39][40][41][42][43][44][45][46][47][48][49][50][51][52][53] due to loss of molecular water with DTA peaks at 71-134°C. In the case of C-S-HPN material, the decomposition temperature (T d )inthis region is variable depending on the synthesis and material compositions.…”
Section: Tg and Dta Analysis Of C-s-h Pva And C-s-hpn Materialsmentioning
confidence: 99%
“…The shift of DTA peak to the higher temperature in C-S-HPN material compared to pure PVA and C-S-H is due to the improved thermal stability of C-S-HPN material. • Over 550°C: this temperature region is characteristic for structural water and CaCO 3 decomposition [36][37][38][39][40][41][42][43][44][45][46][47][48][49][50][51][52][53]. The atmospheric moisture and CO 2 causes the formation of Ca(OH) 2 and CaCO 3 .…”
Section: Tg and Dta Analysis Of C-s-h Pva And C-s-hpn Materialsmentioning
confidence: 99%