“…Upon to now, many compounds with inorganic structures, organic structures, or inorganic/organic hybrid structures had been employed to investigate their nucleation effect on the crystallization process of PLLA. And the current typical nucleating agents include talc [12,13], montmorillonite [14,15], silicon dioxide [16], calcium carbonate [17,18], phenylphosphonate metals [19,20], metallic phenylmalonate salts [21], 1H-benzotriazole derivatives [22,23], benzoyl hydrazine derivatives [24,25], etc. For examples, upon the addition of 0.5 wt % commercial graphene oxide nanoplatelets, the half-time of crystallization of the PLA stereocomplex lower to around 5.5 min at 165°C [26].…”