“…Thus, the obtained DE value of 0.281 eV for l ex = 377 nm is greater than that of 0.156 eV for l ex = 349 nm, and both are comparable to those of several previously reported Bi 3+ /Tb 3+ /Eu 3+ co-doped phosphors, such as Ca 2.24 ZrSi 2 -O 9 :0.17Eu 3+ , 0.09Bi 3+ , 0.50Tb 3+ (DE = 0.195 eV), Gd 1.474 MoB 2 -O 9 :0.30Bi 3+ , 0.20Tb 3+ , 0.026Eu 3+ , (DE = 0.17 eV) and LaMoBO 6 :0.4Tb 3+ , 0.005Eu 3+ , 0.02Bi 3+ (DE = 0.19 eV). 30,31,71 This phosphor exhibits strong temperature sensitization when excited at 377 nm, and its CIE coordinates shi signicantly from (0.4540, 0.4052) to (0.2891, 0.3308) as the temperature increases from 303 to 483 K, indicating its potential application in temperature sensing. Fig.…”