Abstract:The twin-roll casting (TRC) of light metal alloys, in particular aluminium and magnesium alloys, represents a promising technology for the production of lightweight components thanks to its short process chain and promising combinations of properties. In the production of strip products, TRC is susceptible to a number of defects due to the coupled process steps of casting and forming, which prevent its use for more complex alloy combinations in the field. In this review, the defects in TRC of light metal alloy… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.