Welding Defect and Mechanical Properties of Nanosecond Laser Cleaning 6005A Aluminum Alloy

Abstract: Nanosecond laser cleaning effectively removes oxide film and dirt from the surface of aluminum body parts for rail transit, as well as improving surface properties. The effect of laser cleaning on the quality of weld was studied in detail for different scanning frequencies and cleaning speeds. The effect of post-weld laser cleaning on weld quality was investigated. After laser cleaning at different parameters, the surface oxygen content was decreased and the surface roughness and surface hardness were increase… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Year Published

2024
2024
2024
2024

Publication Types

Select...
2
1

Relationship

0
3

Authors

Journals

citations
Cited by 3 publications
references
References 31 publications
0
0
0
Order By: Relevance