A green strategy toward extraction of cadmium(II) during the transformation from arsenic-rich flue dust to scorodite

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 13 publications
(1 citation statement)
references
References 33 publications
0
1
0
Order By: Relevance
“…Hydrogen peroxide (H 2 O 2 ) solution can be used as the leaching agent and oxidizing agent for Cd leaching. H 2 O 2 leaching of As-rich dust with a Cd content of 5.78% produced from the Te smelting process indicated that the Cd leaching rate was 84.3% under the conditions of an H 2 O 2 dosage of 34.5 mL/L, a liquid-to-solid ratio of 5:1 mL/g, and a leaching time of 5 h [60]. The dust with a Cd content of 16.86% produced by a Pb and Zn smelting enterprise in Yunnan Province, China, was dissolved in a mixed H 2 SO 4 and H 2 O 2 solution.…”
Section: Hydrogen Peroxide Solution Leachingmentioning
confidence: 99%
“…Hydrogen peroxide (H 2 O 2 ) solution can be used as the leaching agent and oxidizing agent for Cd leaching. H 2 O 2 leaching of As-rich dust with a Cd content of 5.78% produced from the Te smelting process indicated that the Cd leaching rate was 84.3% under the conditions of an H 2 O 2 dosage of 34.5 mL/L, a liquid-to-solid ratio of 5:1 mL/g, and a leaching time of 5 h [60]. The dust with a Cd content of 16.86% produced by a Pb and Zn smelting enterprise in Yunnan Province, China, was dissolved in a mixed H 2 SO 4 and H 2 O 2 solution.…”
Section: Hydrogen Peroxide Solution Leachingmentioning
confidence: 99%