A new strategy to realize phase structure and morphology of BaTiO3 nanowires controlled in ZnO-B2O3-SiO2 glass

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2

Citation Types

0
2
0

Year Published

2022
2022
2023
2023

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(2 citation statements)
references
References 27 publications
0
2
0
Order By: Relevance
“…The good wettability was exhibited between the glass frit of ZnO–B 2 O 3 –SiO 2 and the surface of BaTiO 3 ceramics, which did not react with the BaTiO 3 substrate to form a second phase. Nevertheless, the low coefficient of thermal expansion (CTE) of glass was mismatched with the CTE of copper powder, which was sensitive to crack during the sintering process 13,14 . An alternative glass system of BaO–B 2 O 3 –SiO 2 has been proposed in previous studies, which was provided a close CTE to the substrate material and low T g , but if the content of BaO was high enough that would lead to phase separation and poor chemical stability 15,16 .…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…The good wettability was exhibited between the glass frit of ZnO–B 2 O 3 –SiO 2 and the surface of BaTiO 3 ceramics, which did not react with the BaTiO 3 substrate to form a second phase. Nevertheless, the low coefficient of thermal expansion (CTE) of glass was mismatched with the CTE of copper powder, which was sensitive to crack during the sintering process 13,14 . An alternative glass system of BaO–B 2 O 3 –SiO 2 has been proposed in previous studies, which was provided a close CTE to the substrate material and low T g , but if the content of BaO was high enough that would lead to phase separation and poor chemical stability 15,16 .…”
Section: Introductionmentioning
confidence: 99%
“…Nevertheless, the low coefficient of thermal expansion (CTE) of glass was mismatched with the CTE of copper powder, which was sensitive to crack during the sintering process. 13,14 An alternative glass system of BaO-B 2 O 3 -SiO 2 has been proposed in previous studies, which was provided a close CTE to the substrate material and low T g , but if the content of BaO was high enough that would lead to phase separation and poor chemical stability. 15,16 An optimized ZBS glass frit composition should meet requirements of not only high CTE, low T g , and good wettability for terminal electrode paste, but also electrical conductivity and acid resistance during copper electroplating processes that was implemented next to the terminal electrode built up.…”
Section: Introductionmentioning
confidence: 99%