Abstract: A wearable, low-cost, highly repeatable piezoresistive sensor was fabricated by the synthesis of modified-graphite and polyurethane (PU) composites and polydimethylsiloxane (PDMS). Graphite sheets functionalized by using a silane coupling agent (KH550) were distributed in PU/N,N-dimethylformamide (DMF) solution, which were then molded to modified-graphite/PU (MG/PU) composite films. Experimental results show that with increasing modified-graphite content, the tensile strength of the MG/PU films first increased… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
24
0

Year Published

2018
2018
2022
2022

Publication Types

Select...
8

Relationship

1
7

Authors

Journals

citations
Cited by 38 publications
(27 citation statements)
references
References 41 publications
0
24
0
Order By: Relevance
“…The piezoresistive sensitivity of the composites can be expressed as the following formula [ 32 ]: ∆P is the relative loaded compressive force, R 0 is initial resistance and R is the resistance. Table 3 summarizes the sensitivity of the composites under varying applied pressures.…”
Section: Resultsmentioning
confidence: 99%
“…The piezoresistive sensitivity of the composites can be expressed as the following formula [ 32 ]: ∆P is the relative loaded compressive force, R 0 is initial resistance and R is the resistance. Table 3 summarizes the sensitivity of the composites under varying applied pressures.…”
Section: Resultsmentioning
confidence: 99%
“…Some of the commonly studied elastomers included polyvinylidene fluoride (PVDF) [10], polyurethanes [9,11], styrene-butadiene rubber [12] and natural rubber latex or natural rubber [9,13]. In current research, GO modified elastomer has been developed by different groups [8][9][10][11][12][13][14][15], they were mainly synthesized by traditional methods such as melt mixing [8], solution/latex blending [8,9,11,12], in-situ polymerization [8], and film processing [10,13]. The GO modified elastomers showed stronger mechanical properties than the corresponding pure elastomers [13,15].…”
Section: Introductionmentioning
confidence: 99%
“…The piezoresistive sensitivity of the TPU/CNT sensing elements can be expressed by the following formula [29]:…”
Section: Piezoresistive Sensitivitymentioning
confidence: 99%