A Review of Capacity Fade Mechanism and Promotion Strategies for Lithium Iron Phosphate Batteries
Chen Hu,
Mengmeng Geng,
Haomiao Yang
et al.
Abstract:Commercialized lithium iron phosphate (LiFePO4) batteries have become mainstream energy storage batteries due to their incomparable advantages in safety, stability, and low cost. However, LiFePO4 (LFP) batteries still have the problems of capacity decline, poor low-temperature performance, etc. The problems are mainly caused by the following reasons: (1) the irreversible phase transition of LiFePO4; (2) the formation of the cathode–electrolyte interface (CEI) layer; (3) the dissolution of the iron elements; (4… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.