“…This undesirable phenomenon occurs during post-weld heat treatment and involves catastrophic growth of a few grains which finally consume almost entire weld zone. It has been observed in various aluminum alloys including 1 xxx [3][4][5][6], 2 xxx [7][8][9][10][11][12][13][14][15][16], 5 xxx [17][18][19][20][21][22][23][24][25][26][27][28][29], 6 xxx [30][31][32][33], and 7 xxx [11,[34][35][36][37][38][39][40][41] series, as well as in magnesium alloys [42][43][44][45], some steels [46][47][48][49], and even metal-matrix composites [50,…”