“…In order to further improve SSA, Shu, et al [10] introduced a short-term NaOH treat-ment on the pre-calcined halloysite, and then etched it with acid, producing mesoporous silica nanotubes with SSA as high as 608 m 2 /g. Nevertheless, the SSA is still limited compared to those of the mesoporous silica fabricated by the traditional template methods (700 m 2 /g-1000 m 2 /g) for FDU-1 [11] , SBA-15 [12] , KIT-6 [13] . Thus, it is still of urgency to develop new processes for preparing halloysite-derived mesoporous silica with further improved SSA.…”