Amino-acid-assisted preparation of CoAl2O4/kaolin hybrid pigments

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
0
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 37 publications
0
0
0
Order By: Relevance
“…In the range from 240 to 310 °C, the stair of weight loss indicates the transformation of precursors to the crystal phase [32]. From the relative DSC curve, a specific exothermic peak occurs at 282 °C, probably related to the burning of ethanol [33].…”
Section: Crystal Phases After Heat Treatment At Different Temperaturesmentioning
confidence: 99%
“…In the range from 240 to 310 °C, the stair of weight loss indicates the transformation of precursors to the crystal phase [32]. From the relative DSC curve, a specific exothermic peak occurs at 282 °C, probably related to the burning of ethanol [33].…”
Section: Crystal Phases After Heat Treatment At Different Temperaturesmentioning
confidence: 99%