“…Then, by adding 5, 10, and 15% vanadium we expect to form alloys residing within the a phase, a plus (Cr, V), and a plus r phase region as indicated by the circles in Finally, for the case of 10% Cr and 10% V carbon has been added with concentrations of 0.2% and 0.4%. This should lead to pronounced carbide formation as investigated and described in [4] and might result in a further increase in hardening. The resulting five different Fe-Cr-V alloys/steels are listed in Table 1.…”