1996
DOI: 10.1016/0020-7683(95)00033-7
|View full text |Cite
|
Sign up to set email alerts
|

Analysis of Berkovich indentation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

3
187
0
1

Year Published

2001
2001
2017
2017

Publication Types

Select...
4
4

Relationship

0
8

Authors

Journals

citations
Cited by 328 publications
(196 citation statements)
references
References 0 publications
3
187
0
1
Order By: Relevance
“…(4) and are referred to as "microhardness." Provided hardness is consistently reported in the same units and with the area calculated in the same manner, measurements made with Berkovich and Vickers indenters are found to have quite good agreement, largely due to the fact that both indenters are selfsimilar with a nearly identical relationship between projected area and indentation depth [5,34,35].…”
Section: Microindentation Testingmentioning
confidence: 61%
See 2 more Smart Citations
“…(4) and are referred to as "microhardness." Provided hardness is consistently reported in the same units and with the area calculated in the same manner, measurements made with Berkovich and Vickers indenters are found to have quite good agreement, largely due to the fact that both indenters are selfsimilar with a nearly identical relationship between projected area and indentation depth [5,34,35].…”
Section: Microindentation Testingmentioning
confidence: 61%
“…Vickers hardness, VH, was calculated by dividing the applied force (in kg) by the indent surface area (in mm 2 ) [5] in the standard manner. However, for a comparison between the nanohardness, the Vickers hardness were converted to the units of GPa and a hardness, H micro , based on a projected contact area of the Vickers indenter [5,17,34,35]:…”
Section: Microindentation Testingmentioning
confidence: 99%
See 1 more Smart Citation
“…but there are no exact analytical expressions for pyramidal tip indentation. Numerical studies [6,7] have suggested that a correction factor 1.034 should be used to correct the modulus values predicted from conical tip to match the results obtained from a pyramidal tip. 20 (2002) [806][807][808][809][810] The indentation modulus of an anisotropic material in any direction can be predicted by using its anisotropic elastic constants.…”
Section: Tlieoreticul Methodsmentioning
confidence: 99%
“…Generally, finite element (FE) simulations have been shown to be a powerful tool for more sophisticated analyses and can be used to extract quantitative information on the stress-strain behaviour from nanoindentation data [7][8][9][10]. Also, FE methods combined with dimensional analysis have been used to extract mechanical properties of materials [11][12][13] and scaling relationships for indentation were determined [14].…”
Section: Introductionmentioning