Application of the technology of induction chemical-thermal treatment to improve the physical and mechanical properties of tantalum

Abstract: The results of the chemical thermal treatment (CTT) of tantalum in a solid carbon- containing medium in the temperature range from 1000 to 1300 °C were presented. CTT consisted in heating a workpiece with a working medium in a container made of a refractory material. The induction heating method was used for heating. After strengthening treatment, tantalum samples were characterized by increased hardness, which grew from 140 to 1100 HV0.02.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Publication Types

Select...

Relationship

0
0

Authors

Journals

citations
Cited by 0 publications
references
References 4 publications
0
0
0
Order By: Relevance

No citations

Set email alert for when this publication receives citations?