Assessment of chemical, ultrasonic, diode laser, and Er:YAG laser application on debonding of ceramic brackets

Abstract: Background Risk of enamel damage that often accompanies ceramic brackets debonding raises the demand of finding an optimal method for debonding of them without adverse effects. Different techniques were proposed in an attempt to facilitate their debonding. Comparison of these techniques is crucial. The aim of this study was to evaluate and compare different techniques for debonding of ceramic brackets in terms of shear bond strength and adhesive remnant index. Mat… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

2
6
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 8 publications
(8 citation statements)
references
References 50 publications
2
6
0
Order By: Relevance
“…Transbond XT adhesive and paste are one of the standard materials used for bonding in orthodontics and has been the focus of many past studies investigating the SBS [31][32][33][34][35]. In a recent study, the same two-step system was used for bracket bonding and the results in the control group (where Transbond XT was used) showed similar SBS values as those obtained in the present study [36]. We found only one study [37] investigating the selfadhesive system, and it does not show significant difference in the SBS with respect to Transbond XT, which is in agreement with our results.…”
Section: Discussionsupporting
confidence: 78%
“…Transbond XT adhesive and paste are one of the standard materials used for bonding in orthodontics and has been the focus of many past studies investigating the SBS [31][32][33][34][35]. In a recent study, the same two-step system was used for bracket bonding and the results in the control group (where Transbond XT was used) showed similar SBS values as those obtained in the present study [36]. We found only one study [37] investigating the selfadhesive system, and it does not show significant difference in the SBS with respect to Transbond XT, which is in agreement with our results.…”
Section: Discussionsupporting
confidence: 78%
“…Khalil et colab. [ 12 ] used acetone and ethanol at different concentrations to test their ability to dissolve orthodontic adhesive; however, no statistically significant differences were found for shear strength and the residual adhesive index. Even when a longer application time was used, the results did not support their hypothesis.…”
Section: Discussionmentioning
confidence: 99%
“…Despite being aesthetically superior, monocrystalline ceramic brackets have a higher resistance to adhesion to enamel and less to the removal procedure, increasing the risk of fracture due to the low modulus of elasticity, low flexibility, and greater fragility compared to metal brackets [ 12 ].…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…One of the challenges following the completion of orthodontic treatment is the debonding of aesthetic brackets, as this should be achieved without causing enamel damage or discomfort to the patient [ 11 , 12 , 13 , 14 ].…”
Section: Introductionmentioning
confidence: 99%