Assessment of Properties on AISI430 Ferritic Stainless Steel by Nitriding process

Abstract: AISI 430 Ferritic Stainless Steel is well known for its good corrosion resistance applicable for high resistance to pitting and stresses. But it lacks in its wear resistance and hardness in order to improve the mechanical properties of AISI 430 Ferritic Stainless-Steel materials Nitriding Heat Treatment is chosen in this project. The samples are taken in the form of cylindrical shapes with diameter 10mm and length 40mm respectively. The specimen is subjected 4 numbers being the highest treated to saturated lim… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
0
0

Year Published

2021
2021
2023
2023

Publication Types

Select...
10

Relationship

6
4

Authors

Journals

citations
Cited by 25 publications
(5 citation statements)
references
References 13 publications
0
0
0
Order By: Relevance
“…For this research work, austenitic stainless steel AISI 304 were taken and the composition was examined as 10% Nickel, 0.09% Carbon, 1.99% Manganese, 0.79% Silicon, 0.048% Phosphorus, 0.02% Sulfur, 0.09% Nitrogen,19.63% Chromium and remaining is iron [24][25][26][27][28].…”
Section: Composition Of Materialsmentioning
confidence: 99%
“…For this research work, austenitic stainless steel AISI 304 were taken and the composition was examined as 10% Nickel, 0.09% Carbon, 1.99% Manganese, 0.79% Silicon, 0.048% Phosphorus, 0.02% Sulfur, 0.09% Nitrogen,19.63% Chromium and remaining is iron [24][25][26][27][28].…”
Section: Composition Of Materialsmentioning
confidence: 99%
“…The annealing process for AISI 410 typically involves heating the steel to a temperature between 723°C to 950°C, depending on the desired properties, and holding it at that temperature for a period of time, typically between 45 minutes to 3 hours. The steel is then cooled slowly in the furnace to reduce the risk of cracking or warping [23][24][25][26][27].…”
Section: Introductionmentioning
confidence: 99%
“…This allows for the complete transformation of the microstructure from martensite (a hard, brittle phase) to a softer, more ductile phase. The cooling rate can be relatively slow, such as air cooling or furnace cooling, to avoid introducing excessive hardness [23][24][25][26].…”
Section: Introductionmentioning
confidence: 99%