Atomic Layer Deposition of Bismuth Vanadate Core–Shell Nanowire Photoanodes

Abstract: Bismuth vanadate (BVO) is a promising metal oxide semiconductor for photoelectrochemical water oxidation. In this study, BVO was deposited using atomic layer deposition (ALD) of alternating films of bismuth and vanadium oxides. A novel Bi-alkoxide precursor was used to enable precise control of stoichiometry along the spectrum of Bi-rich to V-rich compositions, and phase-pure monoclinic BVO films were obtained after postannealing. A planar photoanode composed of an undoped 41.8 nm BVO thin-film electrode with … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
40
0
1

Year Published

2020
2020
2021
2021

Publication Types

Select...
5

Relationship

1
4

Authors

Journals

citations
Cited by 31 publications
(43 citation statements)
references
References 51 publications
2
40
0
1
Order By: Relevance
“…Ternary oxides can also be deposited using ALD by combining two binary processes into a supercycle. [17][18][19] A supercycle combines and repeats the different binary ALD processes to deposit a multi-component film with the desired composition, as shown in Figure 1a.…”
Section: Introductionmentioning
confidence: 99%
“…Ternary oxides can also be deposited using ALD by combining two binary processes into a supercycle. [17][18][19] A supercycle combines and repeats the different binary ALD processes to deposit a multi-component film with the desired composition, as shown in Figure 1a.…”
Section: Introductionmentioning
confidence: 99%
“…As is expected, and has been widely reported, these results highlight the benefit of forming nanostructured heterojunctions to improve the PEC performance of BiVO 4 photoanodes. [ 28,30,32,37,38,43,44 ]…”
Section: Resultsmentioning
confidence: 99%
“…c‐f) Reproduced with permission. [ 32 ] Copyright 2019, American Chemical Society. g) SEM image of the top view of the nanotubes that were coated by ATO and BiVO 4 using ALD.…”
Section: Light Absorbermentioning
confidence: 99%
“…ALD has been used for the deposition onto the nanowire substrate. [ 32,33 ] With bismuth vanadate, two metal precursors need to be introduced. BiVO 4 is produced by the introduction of Bi‐ and V‐ precursors cycles following thermal annealing, to induce crystallization of Bi‐ and V‐ layers (Figure 3c–f).…”
Section: Light Absorbermentioning
confidence: 99%
See 1 more Smart Citation