“…Application of metal primer is easy and requires no elaborate or high-priced equipments [31,32]. However, results with metal primers were not always satisfactory, because they attained a high bond strength under dry circumstances, but controversial reports came out under intraoral, wet conditions with reference to their hydrolytic stability [12,21,32,33]. In this sense, the current study investigated that as an alternative to sandblasting, the application of metal primers (Alloy primer, V-primer and Metaltite) prior to cementation can provide similar bond strength of resin cements to Y-TZP ceramics after thermocycling.…”