Abstract:Nickel‐based superalloys are unique materials with complex doping that demonstrate excellent resistance to mechanical and chemical degradation. Over a long period of use in industry, a variety of information has been accumulated about their possible chemical compounds and features corresponding to a certain composition. One of the main service properties of the alloy is the tensile strength (σ). For a more convenient comparison of the characteristics of the alloys with different chemical compositions, the temp… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.