2001
DOI: 10.1080/000164702760300297
|View full text |Cite
|
Sign up to set email alerts
|

Calcium phosphate coatings for fixation of bone implants. Evaluated mechanically and histologically by stereological methods

Abstract: Calcium phosphate coatings for fixation of bone implants. Evaluated mechanically and histologically by stereological methods Søren Overgaard To cite this article: Søren Overgaard (2001) Calcium phosphate coatings for fixation of bone implants. Evaluated mechanically and histologically by stereological methods,

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
5
0

Year Published

2007
2007
2023
2023

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 10 publications
(5 citation statements)
references
References 334 publications
(589 reference statements)
0
5
0
Order By: Relevance
“…3,4 Significant loss of the HA coating on both immobilised and continuously loaded implants has been demonstrated in vivo. 5 Fractures between the coating and the Ti6Al4V substrate have been observed after implantation times as short as 12 weeks and as long as one year; 6,7 the primary reason for the failure at the interface is the residual stress due to the mismatch of the coefficients of thermal expansion (CTE) of the ceramic and metal components, which can induce micro-cracking initiating the de-bonding of the coating from the substrate. [8][9][10] The micro-cracking of silicate glass coatings on Ti6Al4V substrates due to mismatch of CTE has also been recorded.…”
Section: Introductionmentioning
confidence: 99%
“…3,4 Significant loss of the HA coating on both immobilised and continuously loaded implants has been demonstrated in vivo. 5 Fractures between the coating and the Ti6Al4V substrate have been observed after implantation times as short as 12 weeks and as long as one year; 6,7 the primary reason for the failure at the interface is the residual stress due to the mismatch of the coefficients of thermal expansion (CTE) of the ceramic and metal components, which can induce micro-cracking initiating the de-bonding of the coating from the substrate. [8][9][10] The micro-cracking of silicate glass coatings on Ti6Al4V substrates due to mismatch of CTE has also been recorded.…”
Section: Introductionmentioning
confidence: 99%
“…Satisfactory to excellent results were reported when adequate stem anchorage was obtained [15,[19][20][21][22].…”
Section: Introductionmentioning
confidence: 99%
“…The SD was set to 50%, and a MIREDIF of 80% was selected. At least six samples per group were needed according to assumptions 36 . To account for dropout, two additional sheep were added, so eight sheep per group were included.…”
Section: Methodsmentioning