One
kind of nylon-610 oligomer (PrePA) was prepared from the reaction
of nylon-610 salt with sebacic acid. Polyesteramide prepolymers (PrePEAs)
having amide content from 10 to 60 mol % were synthesized through
melt polycondensation from adipic acid, 1,4-butanediol, and the PrePA
with the catalysis of stannous chloride. Chain extension of the PrePEAs
was carried out at 210 °C using 2,2′-(1,4-phenylene)-bis(2-oxazoline)
and adipoyl biscaprolactamate as combined chain extenders. The chain
extended polyesteramides (ExtPEAs) with intrinsic viscosity up to
0.70 dL/g were synthesized. The ExtPEAs were characterized by FTIR
and 1H NMR spectrum, differential scanning calorimetry,
wide-angle X-ray scattering, thermogravimetric analysis, tensile test,
and enzymatic degradation. The results showed that the ExtPEAs were
biodegradable and had T
m from 95.20 to
155.67 °C, initial decomposition temperature over 325.3 °C,
and tensile strength up to 33.1 MPa.