Characterization of Microstructures and Mechanical Properties of Cold-rolled Medium-Mn Steels with Different Annealing Processes

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
8
0

Year Published

2017
2017
2023
2023

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 23 publications
(8 citation statements)
references
References 34 publications
0
8
0
Order By: Relevance
“…Many alloying concepts are relying on the effect of transformation-induced plasticity (TRIP) of austenite to achieve the target of high strength and high ductility. Examples include quenching and partitioning steels [3,4], medium manganese TRIP steels [5,6], and lowdensity δ-TRIP steels [7,8]. The metastable austenite transforms gradually into martensite during deformation [3][4][5][6][7][8].…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…Many alloying concepts are relying on the effect of transformation-induced plasticity (TRIP) of austenite to achieve the target of high strength and high ductility. Examples include quenching and partitioning steels [3,4], medium manganese TRIP steels [5,6], and lowdensity δ-TRIP steels [7,8]. The metastable austenite transforms gradually into martensite during deformation [3][4][5][6][7][8].…”
Section: Introductionmentioning
confidence: 99%
“…Examples include quenching and partitioning steels [3,4], medium manganese TRIP steels [5,6], and lowdensity δ-TRIP steels [7,8]. The metastable austenite transforms gradually into martensite during deformation [3][4][5][6][7][8]. The formation of martensite sustains the work hardening and improves the ductility by delaying the necking during deformation [9].…”
Section: Introductionmentioning
confidence: 99%
“…Annealing Conditions Table 3 shows that the concentration of carbon in austenite (C γ ) decreases with increasing in annealing time, presumably because this behavior is paralleled by an increase in the γ volume fraction (γ R ). The product of these two values (γ R × C γ ) 39) serves as an index of the degree to which the carbon dissolved in the steel is localized within the austenite: its maximum value (0.1) derives from its compositional weight (0.1%). 40) The γ R × C γ of UFG ferrite-austenite steels ranges from 0.033-0.057 when obtained from M, suggesting a large proportion of the carbon remained dissolved in martensite matrix.…”
Section: Change In Austenite Stability With Intercriticalmentioning
confidence: 99%
“…And the batch annealing is not possible to account for the accuracy of the temperature profile in practice. The Mn-TRIP steels are developing by the other microstructure evolution that manganese partitioning during the transformation from severe deformed martensite and short isothermal holding within several minutes [45,[47][48][49]. This could be applied for commercial available continuous annealing lines (CAL) with temperature tolerance less than ±10°C.…”
Section: Mn-tripmentioning
confidence: 99%