2018
DOI: 10.1039/c7nj04138a
|View full text |Cite
|
Sign up to set email alerts
|

Chemical coatings relying on the self-polymerization of catechol for retrievable vena cava filters

Abstract: After covalent conjugation with catechol, heparin and paclitaxel can be chemically coated on a Ti–Ni alloy to endow anti-thrombosis and anti-intimal hyperplasia properties, respectively.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(3 citation statements)
references
References 30 publications
0
3
0
Order By: Relevance
“…The disappearance of peaks at 3013 and 946 cm –1 (Figure c), assigned to the stretching vibrations of the unsaturated group in the side chain of UH, implies a cross-linking reaction in the side chain . The absorption peak at 2927 cm –1 increased upon the introduction of UH into the hydrogels (Figure d), corresponding to the characteristic vibration peak of C–H on the alkyl side chains of UH. , Moreover, the increased intensity of the broad peak at 3250–3350 cm –1 , assigned to the O–H stretching vibration, further indicates the successful introduction of UH into the HBU hydrogels. , …”
Section: Resultsmentioning
confidence: 93%
See 1 more Smart Citation
“…The disappearance of peaks at 3013 and 946 cm –1 (Figure c), assigned to the stretching vibrations of the unsaturated group in the side chain of UH, implies a cross-linking reaction in the side chain . The absorption peak at 2927 cm –1 increased upon the introduction of UH into the hydrogels (Figure d), corresponding to the characteristic vibration peak of C–H on the alkyl side chains of UH. , Moreover, the increased intensity of the broad peak at 3250–3350 cm –1 , assigned to the O–H stretching vibration, further indicates the successful introduction of UH into the HBU hydrogels. , …”
Section: Resultsmentioning
confidence: 93%
“…40 The absorption peak at 2927 cm −1 increased upon the introduction of UH into the hydrogels (Figure 2d), corresponding to the characteristic vibration peak of C−H on the alkyl side chains of UH. 41,42 Moreover, the increased intensity of the broad peak at 3250− 3350 cm −1 , assigned to the O−H stretching vibration, further indicates the successful introduction of UH into the HBU hydrogels. 40,43 We further analyzed the surface chemical composition of the HBU hydrogels via XPS (Figure 2e−i).…”
Section: Characterization Of Hbu Hydrogelsmentioning
confidence: 96%
“…Quantification of surface-bound elements also can be performed, but it is challenging and rarely used. XPS analysis penetration depth is about 10 nm, limiting its use to thin coatings ( Bao et al, 2018 ). You et al examined the XPS nitrogen peak at binding energy of 400 eV to confirm surface coating of exosomes on PLGA cores mediated by polydopamine ( You et al, 2020 ).…”
Section: Characterization Of Surface Modificationmentioning
confidence: 99%