ChemInform Abstract: The Stress Corrosion Crack (SCC) Growth Rate in Sensitized Alloy 600 in Thiosulfate Solution.

Abstract: The Stress Corrosion Crack (SCC) Growth Rate in Sensitized Alloy 600 in Thiosulfate Solution. -The effect of the applied potential on the SCC growth rate of sensitized Alloy 600 in 0.01 M Na2S2O3 solution at 25 • C is studied by a constant deflection technique using precracked samples. With increasing applied potential in the anodic passive region the intergranular SCC growth rate increases while the critical stress intensity factor for SCC (KISCC) decreases. At +500 mV in the transpassive potential region a r… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Publication Types

Select...

Relationship

0
0

Authors

Journals

citations
Cited by 0 publications
references
References 1 publication
0
0
0
Order By: Relevance

No citations

Set email alert for when this publication receives citations?