Chloride-Induced Stress Corrosion Cracking of Friction Stir-Welded 304L Stainless Steel: Effect of Microstructure and Temperature
Anirban Naskar,
Madhumanti Bhattacharyya,
Saumyadeep Jana
et al.
Abstract:Dry storage canisters of used nuclear fuels are fabricated using SUS 304L stainless steel. Chloride-induced stress corrosion cracking (CISCC) is one of the major failure modes of dry storage canisters. The cracked canisters can be repaired by friction stir welding (FSW), a low-heat input ‘solid-phase’ welding process. It is important to evaluate the ClSCC resistance of the friction stir welded material. Stress corrosion cracking (SCC) studies were carried out on mill-annealed base materials and friction stir w… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.