Comparison of four monolithic zirconia materials with conventional ones: Contrast ratio, grain size, four-point flexural strength and two-body wear

Abstract: OBJECTIVES: To test the mechanical and optical properties of monolithic zirconia in comparison to conventional zirconia. MATERIALS AND METHODS: Specimens were prepared from: monolithic zirconia: Zenostar (ZS), DD Bio ZX2 hochtransluzent (DD), Ceramill Zolid (CZ), InCoris TZI (IC) and a conventional zirconia Ceramill ZI (CZI). Contrast ratio (N=75/n=15) was measured according to ISO 2471ISO :2008. Grain sizes (N=75/n=15) were investigated with scanning electron microscope. Fourpoint flexural strength (N=225/n=… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

11
113
2
15

Year Published

2017
2017
2023
2023

Publication Types

Select...
6
1
1

Relationship

0
8

Authors

Journals

citations
Cited by 129 publications
(141 citation statements)
references
References 28 publications
11
113
2
15
Order By: Relevance
“…39 Thus, the increased resistance to hydrothermal degradation after grinding is possibly related to the existence of this very thin layer of tetragonal recrystallized nano-grains (10-20 nm) that are smaller than the critical size for transformation in humid environment, in addition to the presence of residual compressive stress on the surface of Y-TZP ceramics. 39,40 Although the tested Y-TZP ceramic consists of a new translucent material, and therefore alterations on microstructure and composition (that are not clearly stated by the manufacturer) may be expected in comparison to conventional Y-TZP ceramics 4 , our data support a similar performance of the tested ceramic to the ones that have been evaluated by previous studies. 15,16,17,18,19 Finally, we showed that the protocols for grinding and aging used by this study do not promote a deleterious effect on the mechanical properties of Y-TZP ceramic, regardless of the ceramic thickness.…”
Section: Discussionsupporting
confidence: 78%
See 1 more Smart Citation
“…39 Thus, the increased resistance to hydrothermal degradation after grinding is possibly related to the existence of this very thin layer of tetragonal recrystallized nano-grains (10-20 nm) that are smaller than the critical size for transformation in humid environment, in addition to the presence of residual compressive stress on the surface of Y-TZP ceramics. 39,40 Although the tested Y-TZP ceramic consists of a new translucent material, and therefore alterations on microstructure and composition (that are not clearly stated by the manufacturer) may be expected in comparison to conventional Y-TZP ceramics 4 , our data support a similar performance of the tested ceramic to the ones that have been evaluated by previous studies. 15,16,17,18,19 Finally, we showed that the protocols for grinding and aging used by this study do not promote a deleterious effect on the mechanical properties of Y-TZP ceramic, regardless of the ceramic thickness.…”
Section: Discussionsupporting
confidence: 78%
“…3,4 The major advantage of monolithic restorations is that they allow a substantial reduction of ceramic thickness by eliminating Rodrigo Diniz PRADO (a) Gabriel Kalil Rocha PEREIRA (b) Marco Antonio BOTTINO (a) Renata Marques de MELO (a) Luiz Felipe VALANDRO (b) the veneer layer without compromising the final strength of the system. Thus, this assembly results in a more conservative tooth preparation and decreased removal of tooth structure.…”
Section: Introductionmentioning
confidence: 99%
“…Considering the thickness of 0.5 mm, traditional Y-TZP shows contrast ratio (CR) values that are higher (0.77) than those of monolithic Y-TZPs (0.57 to 0.62). 13 In addition to the mechanical and optical properties, another important characteristic for the long-term success of a restoration is the wear of the antagonist enamel and the marginal adaptation. Fortunately, laboratory studies have shown that monolithic zirconia usually causes a rather comparable wear of the antagonists in comparison to other restorative ceramics, and this wear rate is within the physiological range reported in the literature.…”
Section: Monolithic Zirconia Restorationsmentioning
confidence: 99%
“…Some of these studies compared different surface finishing techniques for monolithic zirconia restorations, such as polishing versus glazing, and found that polished surfaces resulted in less enamel wear of the antagonist. 13,14,15,16 It is needless to say that the high surface hardness of zirconia has a major influence on the antagonist wear and a perfect polish of any monolithic zirconia restoration is therefore very important. A clinical study evaluated the occlusal surface wear of monolithic zirconia crowns placed in premolars and molars.…”
Section: Monolithic Zirconia Restorationsmentioning
confidence: 99%
“…Por outro lado, uma pressão excessiva pode introduzir defeitos na microestrutura do material e também induzir uma não uniformidade da densidade ao longo do bloco. Existem evidências na literatura mostrando que defeitos originados durante a prensagem são frequentemente a origem da fratura de estruturas de Y-TZP para uso dentário (31)(32)(33)(34)(35)(36).…”
Section: Introductionunclassified