“…PP/PAs blends, unfortunately, are immiscible and incompatible through the whole composition range due to their polar/nonpolar character, giving rise to unviable materials for practical use. For this reason, reactive compatibilization, for instance, has been widely used in these blends, where compatibilizing agents such as maleic anhydride (MA), 3,6,10,[13][14][15][16][17][18][19][20][21][22][23][24][25][26][27][28][29][30][31] acrylic acid (AA), 6,24,29,[31][32][33][34] or glycidyl methacrylate (GMA) 26,[35][36][37] linked to the PP have been used. These groups are able to react with the terminal amine groups in the PA, producing a graft copolymer which locates at the interface.…”