Abstract:Superalloys have basic elements like Fe, Ni and Co, the principal applications are in the hottest zones of turborreactors, nuclear reactors, petrochemical equipment and rockets. The aim of this paper is analysing the corrosion resistance of these superalloys in acid electrolytes using electrochemical noise technique. Superalloys evaluated was Waspaloy and Ultimet in H2SO4 and NaCl at 3.5% with two different temperatures, 25 and 60°C. Electrochemical noise technique monitored 1024 data per seconds, obtaining el… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.