Creation of a new material stream from Japanese cedar resources to cellulose nanofibrils

Abstract: a b s t r a c tJapanese cedar is one of the most abundant plantation softwoods in Japan, although it is not effectively utilized as a wood resource. Japanese cedar cellulose was isolated and subjected to one-pot catalytic oxidation and reduction with 2,2,6,6-tetramethylpiperidine-1-oxyl (TEMPO) and NaBH 4 , respectively. The TEMPO-oxidized and NaBH 4 -reduced Japanese cedar celluloses (TOCs-NaBH 4 ) had carboxylate content of up to 1.4 mmol/g and viscosity-average degrees of polymerization from 2000 to 3000. T… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
10
0

Year Published

2016
2016
2021
2021

Publication Types

Select...
5
1

Relationship

3
3

Authors

Journals

citations
Cited by 17 publications
(10 citation statements)
references
References 29 publications
0
10
0
Order By: Relevance
“…The largest thickness along each individual fibril was taken as the true fibril thickness, and the arithmetic mean thicknesses d a and weighted mean thicknesses d w of the NFCs were then calculated in the same way as the L a and L w values, respectively. The neutral sugar compositions of the NFC samples were determined using a high-performance liquid chromatography system at 50 °C . The X-ray diffraction (XRD) patterns of the NFC samples were recorded by the reflection method using a Rigaku RINT 2000 instrument with monochromator-filtered Cu Kα radiation (λ = 0.15418 nm) at 40 kV and 40 mA, and the crystal thicknesses d c of the (2 0 0) plane were calculated using Scherrer’s equation …”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…The largest thickness along each individual fibril was taken as the true fibril thickness, and the arithmetic mean thicknesses d a and weighted mean thicknesses d w of the NFCs were then calculated in the same way as the L a and L w values, respectively. The neutral sugar compositions of the NFC samples were determined using a high-performance liquid chromatography system at 50 °C . The X-ray diffraction (XRD) patterns of the NFC samples were recorded by the reflection method using a Rigaku RINT 2000 instrument with monochromator-filtered Cu Kα radiation (λ = 0.15418 nm) at 40 kV and 40 mA, and the crystal thicknesses d c of the (2 0 0) plane were calculated using Scherrer’s equation …”
Section: Methodsmentioning
confidence: 99%
“…The neutral sugar compositions of the NFC samples were determined using a high-performance liquid chromatography system at 50 °C. 54 The X-ray diffraction (XRD) patterns of the NFC samples were recorded by the reflection method using a Rigaku RINT 2000 instrument with monochromator-filtered Cu Kα radiation (λ = 0.15418 nm) at 40 kV and 40 mA, 8 and the crystal thicknesses d c of the (2 0 0) plane were calculated using Scherrer's equation. 55 ■ RESULTS AND DISCUSSION Characterization of NFCs.…”
Section: ■ Materials and Methodsmentioning
confidence: 99%
“…The chemical methods are to introduce charged groups on cellulose fibrils, and use the repulsion force between the same charges to obtain the separation of nanofibrils. Among them, the common and effective method is 2,2,6,6‐tetramethylpiperidinyl‐1‐oxyl (TEMPO)‐catalyzed oxidation 40 . The TEMPO‐oxidized cellulose nanofibril (TOCN) contains a large amount of carboxylic acid on the surface, and the monodisperse cellulose nanofibril is realized by the repulsion between the same charges 41 .…”
Section: Introductionmentioning
confidence: 99%
“…Preparation of aqueous TOCN dispersion and ionic solution TEMPO-oxidized cellulose (TOC) was prepared by the TEMPO/NaBr/NaClO system with NaClO content of 5.0 mmol g − 1 -cellulose in aqueous solution at pH 10 followed by addition of 1 wt% NaBH 4 to convert the small amounts of C6-aldehydes and C2/C3-ketones to be complete hydroxyl groups following the previously reported method (Shi et al 2015;Takaichi et al 2014). The obtained TOC was washed with deionized water until neutral.…”
Section: Methodsmentioning
confidence: 99%