Cyclic fatigue behavior of Si3N4 ceramics

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
10
0
1

Year Published

1992
1992
2013
2013

Publication Types

Select...
3
3
1

Relationship

0
7

Authors

Journals

citations
Cited by 41 publications
(11 citation statements)
references
References 3 publications
0
10
0
1
Order By: Relevance
“…[43,[103][104][105][106] A rare exception is the data of NGK Insulators Ltd. on their silicon nitride material. [107] It follows from the reported cyclic fatigue data that there also exists a Paris law for cyclic fatigue crack growth. The crack growth per load cycle is…”
Section: Influence Of Fatigue Crack Growth On Strengthmentioning
confidence: 98%
“…[43,[103][104][105][106] A rare exception is the data of NGK Insulators Ltd. on their silicon nitride material. [107] It follows from the reported cyclic fatigue data that there also exists a Paris law for cyclic fatigue crack growth. The crack growth per load cycle is…”
Section: Influence Of Fatigue Crack Growth On Strengthmentioning
confidence: 98%
“…shows the results of cyclic fatigue tests at room temperature, in which tensile specimens and tapered cantilever beam specimens of sintered silicon nitrides were used (Masuda et al, 1990 limit of both specimens with different volumes seem to be the same. Cyclic fatigue strength at elevated temperatures is described next.…”
Section: Cyclic Fatigue Strengthmentioning
confidence: 99%
“…10-43 suggests a decrease in the fatigue limit to about 40% of its initial strength. Figure 10-45 shows the mean stress/ stress amplitude diagram of sintered silicon nitrides (Masuda et al 1990). a t on the horizontal axis represents the mean tensile strength of 6 mm diameter button-head type specimens.…”