1996
DOI: 10.1021/bk-1996-0634.ch004
|View full text |Cite
|
Sign up to set email alerts
|

Deactivation of Zeolite Catalysts by Coke

Abstract: Zeolite catalysts are widely used in conversion processes of hydrocarbons, because of their high activity and shape selectivity. The conversion rate and the shape selectivity are closely related to intracrystalline diffusion rate and acidic properties of the zeolite catalyst. Carbonaceous materials called coke deposit on the catalyst during reactions, leading to changes in catalytic properties (diffusivity and acidic properties) as well as the reaction performance. This presentation reviews the mechanisms of t… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
3
0

Year Published

1998
1998
2020
2020

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 8 publications
(3 citation statements)
references
References 20 publications
0
3
0
Order By: Relevance
“…6c) due to selective removal of Al species (working as Brønsted or Lewis acid sites) on the external surface of the ZSM-5 particles. In paraffin cracking over ZSM-5 zeolite catalysts, it is well-known that the external acid sites give rise to deactivation due to coke formation on these sites, [33][34][35][36] although large 12R micropores of zeolite beta catalysts during catalytic ethanol transformation would induce the formation of coke precursors, such as alkylbenzenes, alkylnaphthalenes and alkylpyrenes. 37 Since Lewis acid sites tend to cause the dehydrogenation of hydrocarbons and related reactions leading to the formation of coke species mainly consisting of polyaromatic compounds, selective leaching of external Lewis acid sites in the ZSM-5 catalyst could lead to diminution of coke formation to give a long-lived catalyst.…”
Section: Catalysis Science and Technology Papermentioning
confidence: 99%
“…6c) due to selective removal of Al species (working as Brønsted or Lewis acid sites) on the external surface of the ZSM-5 particles. In paraffin cracking over ZSM-5 zeolite catalysts, it is well-known that the external acid sites give rise to deactivation due to coke formation on these sites, [33][34][35][36] although large 12R micropores of zeolite beta catalysts during catalytic ethanol transformation would induce the formation of coke precursors, such as alkylbenzenes, alkylnaphthalenes and alkylpyrenes. 37 Since Lewis acid sites tend to cause the dehydrogenation of hydrocarbons and related reactions leading to the formation of coke species mainly consisting of polyaromatic compounds, selective leaching of external Lewis acid sites in the ZSM-5 catalyst could lead to diminution of coke formation to give a long-lived catalyst.…”
Section: Catalysis Science and Technology Papermentioning
confidence: 99%
“…Such a harsh environment can often structurally damage the zeolite by dealumination, structural alteration, sintering of supported metals, etc. (Guisnet, 1995;Masuda, 1995).…”
Section: Introductionmentioning
confidence: 99%
“…20 hrs)·pores. Theref~re a great deal of the existing coke should be located on the catalyst surface thereby resulting in the high stability of ZSM-5 in comparison to other zeolites(Masuda, 1995). (b) Perhaps the only evidence of deactivation, aside from the deposition of coke in the catalyst pores, is the change in concentration of the different hydrocarbon I , product species.…”
mentioning
confidence: 99%