Degradation Resistance of Cordierite Diesel Particulate Filters to Diesel Fuel Ash Deposits

Abstract: The thermochemical degradation resistance of a typical cordierite diesel particulate filter (DPF) material by synthetic ashes typical of those arising in practice has been investigated over the temperature range 950°C–1250°C. Differential thermal analyses and heat treatment of pressed pellets were used to characterize the melting/transformation behavior of ashes representative of typical diesel fuel (ash A) and those typical of when the catalysts ferrocene (ash FeA) and cerium carboxylate (ash CeA) were presen… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Year Published

2014
2014
2021
2021

Publication Types

Select...
4
1

Relationship

0
5

Authors

Journals

citations
Cited by 12 publications
references
References 14 publications
0
0
0
Order By: Relevance