2006
DOI: 10.1016/j.jeurceramsoc.2005.03.261
|View full text |Cite
|
Sign up to set email alerts
|

Densification, microstructural evolution and dielectric properties of Ba6−3x(Sm1−yNdy)8+2xTi18O54 microwave ceramics

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

1
10
0

Year Published

2009
2009
2017
2017

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 30 publications
(11 citation statements)
references
References 27 publications
1
10
0
Order By: Relevance
“…Typical microwave ceramics are included, e.g. MgTiO 3 10,53,54 , BaTi 4 O 9 55 , Ba 6-3x Nd 8+2x Ti 18 O 54 4,30,48 , TiO 2 6,8,9,13,15,56,57 , CaTiO 3 11,14,16,22,24,49,50,58,59 , and Li 1/2 Nd 1/2 TiO 3 17,20,22 . These 3 groups are: 1. multiphase composites, 2. single phase solid solutions, 3. equivalent ionic substituted single phase ceramics.…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…Typical microwave ceramics are included, e.g. MgTiO 3 10,53,54 , BaTi 4 O 9 55 , Ba 6-3x Nd 8+2x Ti 18 O 54 4,30,48 , TiO 2 6,8,9,13,15,56,57 , CaTiO 3 11,14,16,22,24,49,50,58,59 , and Li 1/2 Nd 1/2 TiO 3 17,20,22 . These 3 groups are: 1. multiphase composites, 2. single phase solid solutions, 3. equivalent ionic substituted single phase ceramics.…”
Section: Resultsmentioning
confidence: 99%
“…As the substitution molar ratio increases, the microstructure or the parameters of the original molecular will systemically change. Therefore, the quality factor versus the substitution content is currently attributed to interfacial mismatch 44 , mode vibration 35,58 , phase constitution 45,50 , relative density 46 , grain size 47 , dielectric constant 48 , and crystal structure 59 etc . The interfacial mismatch can be related to grain size which corresponds to the two-dimensional defect leading to the dielectric loss 44 .…”
Section: Resultsmentioning
confidence: 99%
“…The amount of Nd 2 Ti 2 O 7 phase formed increased but the BNBT phase decreased with increasing BB45SZ. Wang et al [11] also reported that a minor pyrochlore (Sm,Nd) 2 Ti 2 O 7 phase was observed during preparing Ba 4.5 (Sm 0.5 Nd 0.5 )Ti 18 O 54 ceramics. Fig.…”
Section: Methodsmentioning
confidence: 98%
“…A dielectric constant of 19.3, a quality factor (Q 9 f) of 43,300 GHz, and a temperature coefficient of resonant frequency of -57 ppm/°C were obtained when Nd(Mg 0.5 Sn 0.5 )O 3 ceramics were sintered at 1,550°C for 4 h [10]. Since several solid solutions combining two compounds were found to have a higher value of Q 9 f compared with that of both end members [11][12][13] and the ionic radius of Zn 2? (0.074 nm) is similar to that of Mg 2?…”
Section: Introductionmentioning
confidence: 99%