2008
DOI: 10.1016/j.porgcoat.2007.09.037
|View full text |Cite
|
Sign up to set email alerts
|

Development of waterborne UV-A curable clear coat for car refinishes

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
11
0

Year Published

2011
2011
2021
2021

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 31 publications
(11 citation statements)
references
References 5 publications
0
11
0
Order By: Relevance
“…8A . To determine the properties of these novel bio-based materials, we subjected the coatings to standardized spot tests to reveal the resistances against water and solvent ( 43 , 44 ). The Persoz hardness test was used to establish the hardness, and the glass transition temperatures and cross-link densities were measured by dynamic mechanical thermal analysis (DMTA).…”
Section: Resultsmentioning
confidence: 99%
“…8A . To determine the properties of these novel bio-based materials, we subjected the coatings to standardized spot tests to reveal the resistances against water and solvent ( 43 , 44 ). The Persoz hardness test was used to establish the hardness, and the glass transition temperatures and cross-link densities were measured by dynamic mechanical thermal analysis (DMTA).…”
Section: Resultsmentioning
confidence: 99%
“…In WPU dispersions, it is possible to obtain the ideal viscosity for the application, because the viscosity of dispersions is generally independent of the molecular weight of the polymer, it will depend on the particles size and the amount of solids present in the dispersion [126,127,167]. The rheological behavior of WPU dispersions belongs to pseudoplastic fluids [11,82,92,130,145].…”
Section: Dispersion Processmentioning
confidence: 99%
“…As expected, when increasing the grafting percentage (from MAH/AGE = 15/23 to 67/81), the glass transition temperature increases (from 75 to 140 °C), because the network was more compact, with a higher crosslinking density. In comparison, in the case of most UV waterborne coatings (polyurethanes), the observed glass transition temperatures can reach 70 °C to 100 °C …”
Section: Resultsmentioning
confidence: 98%
“…Poly-L-lysine (2 g, 2.9 mmol) and allyl glycidyl ether (1.8 g, 15.6 mmol) and 90 mL of methanol were added in a 250 mL round-bottom flask equipped with a magnetic stirrer bar and left under stirring at room temperature at different reaction times (23,48, 72 h). Also, different ratios allyl glycidyl ether/PLL were tested to study their influence on the grafting rate (AGE/PLL 5 1.2, 2.4, 3.7, 4.8, 6.2) with a reaction time of 48 h. The methanol was then concentrated under vacuum; the dried residue was solubilized in a small volume of methanol, and precipitated in a large volume of ethyl acetate, filtered off (this step was performed twice), and dried under vacuum.…”
Section: Synthesis Of Allyl Grafted Poly-l-lysine (Pll-g-ae)mentioning
confidence: 99%
See 1 more Smart Citation