Diamond-like carbon coating of a pure bioplastic foil

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
32
0
3

Year Published

2013
2013
2022
2022

Publication Types

Select...
5

Relationship

3
2

Authors

Journals

citations
Cited by 30 publications
(35 citation statements)
references
References 23 publications
0
32
0
3
Order By: Relevance
“…The chosen pure bioplastic foil is a composition of 92 % polyhydroxybutyrate (PHB) and 8 % polyhydroxyvalerate (PHV) with a thickness of 50 μm (PHB92/PHV8 biopolymer film, Goodfellow BV301050, already used in [16]). Sheets of the size 100 mm × 255 mm were cut out of the delivered foil.…”
Section: Methodsmentioning
confidence: 99%
See 4 more Smart Citations
“…The chosen pure bioplastic foil is a composition of 92 % polyhydroxybutyrate (PHB) and 8 % polyhydroxyvalerate (PHV) with a thickness of 50 μm (PHB92/PHV8 biopolymer film, Goodfellow BV301050, already used in [16]). Sheets of the size 100 mm × 255 mm were cut out of the delivered foil.…”
Section: Methodsmentioning
confidence: 99%
“…The coating process was performed as described previously [15,16,[18][19][20][21]. In difference to the setup used in [15,16], here six of the trays at a time were placed onto a turntable in a high vacuum chamber. The trays rotated at 2 rpm about a vertical axis in the center of the chamber during the coating process.…”