Abstract:Low thermal conductivity of organic phase change materials (PCMs) for thermal
energy storage systems induces the necessity to apply suitable heat transfer
enhancement techniques for these materials. The purpose of this study was to
improve thermal conductivity of a PCM erythritol by using sodium chloride as
an additive, such that the material can be applied for steam cooking systems
when integrated with solar parabolic trough collectors. In this study,
erythritol-NaCl composites were synthesi… Show more
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.