2019
DOI: 10.1007/s12666-019-01635-x
|View full text |Cite
|
Sign up to set email alerts
|

Direct Leaching of Low-Grade Zinc Oxide Ore Containing High Amounts of Iron and Manganese

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
6
0

Year Published

2020
2020
2022
2022

Publication Types

Select...
4

Relationship

1
3

Authors

Journals

citations
Cited by 4 publications
(6 citation statements)
references
References 13 publications
0
6
0
Order By: Relevance
“…Abdel-Aal 37 showed that the enhancement of the temperature from 40 to 70 °C, the Zn leaching efficiency increased from 70 to about 95%. Previous work conducted by the authors showed that increasing the temperature above 45 °C, increases the leaching efficiency of impurities 5 . Therefore, during the leaching experiments, the temperature was set at 45 °C.…”
Section: Resultsmentioning
confidence: 91%
See 4 more Smart Citations
“…Abdel-Aal 37 showed that the enhancement of the temperature from 40 to 70 °C, the Zn leaching efficiency increased from 70 to about 95%. Previous work conducted by the authors showed that increasing the temperature above 45 °C, increases the leaching efficiency of impurities 5 . Therefore, during the leaching experiments, the temperature was set at 45 °C.…”
Section: Resultsmentioning
confidence: 91%
“…In addition, the leaching temperature was set at 45 °C to minimize the leaching efficiency of impurities. The effect of particle size and temperature have been studied in another study by the authors 5 .…”