EAF and LF slag co-processing: Study for wasteless utilization

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2021
2021
2023
2023

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 8 publications
0
1
0
Order By: Relevance
“…The LFS basicity was relatively high for desulfurization, it was set to 2.0 to ensure molten slag and improve the kinetics of the slag–metal reaction. The appropriate amount of Al 2 O 3 was used to significantly reduce the melting temperature, [ 26,27 ] and the necessary quantity of CaF 2 required for destructing the CaS solid to improve the desulfurization conditions [ 28 ] was employed. The Al 2 O 3 and F contents used were therefore 20 and 4 wt%, respectively.…”
Section: Methodsmentioning
confidence: 99%
“…The LFS basicity was relatively high for desulfurization, it was set to 2.0 to ensure molten slag and improve the kinetics of the slag–metal reaction. The appropriate amount of Al 2 O 3 was used to significantly reduce the melting temperature, [ 26,27 ] and the necessary quantity of CaF 2 required for destructing the CaS solid to improve the desulfurization conditions [ 28 ] was employed. The Al 2 O 3 and F contents used were therefore 20 and 4 wt%, respectively.…”
Section: Methodsmentioning
confidence: 99%