Early corrosion properties of titanium alloys, Ni-based alloys and stainless steel in supercritical water oxidation of sewage sludge

Abstract: Supercritical water oxidation (SCWO) can efficiently and harmlessly dispose sewage sludge, while corrosion phenomena can lead to rapid shutdown and/or failure of expensive process equipments in a supercritical water system. The corrosion behavior of titanium alloys, Ni-based alloys and stainless steel exposed in supercritical water oxidation of sewage sludge at 450 °C, 26 MPa for 60 h was investigated by means of gravimetry, scanning electron microscopy, energy dispersive X-ray spectroscopy and X-ray diffracti… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Year Published

2024
2024
2024
2024

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
references
References 11 publications
0
0
0
Order By: Relevance