Objective: To evaluate the long-term color stainability, translucency, and contrast ratio (CR) of different resins used to fabricate interim prostheses after immersion in acidic/staining solutions.
Materials and Methods:A total of 160 specimens were divided into 16 groups (n = 10) according to the material (heat-polymerized acrylic resin [HPAR], autopolymerized acrylic resin [APR], nanoparticulated bis-acrylic resin [BR], and prefabricated poly(methyl methacrylate) block for CAD/CAM [CADR]) and immersion solutions (artificial saliva, cola beverage, coffee, and red wine). A spectrophotometer was used before and after each immersion period (7, 14, 28, 90, and 180 days). Color differences (CIEDE2000 and CIELab) were calculated. A three-way repeatedmeasures analysis of variance and Bonferroni test (α = .05) were used.