Abstract:Abstract. The alumina powder was treated at a high temperature (1000°C). Dense (porosity of less than 2%), solid (1280 ± 30 HV0.3) and wear-resistant coatings based on heat-treated alumina powder were obtained by a multi-chamber detonation sprayer on the steel substrate. The microstructure, microhardness and the wear resistance of the alumina coatings were investigated.
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.