Effect of Mg deficiency on the thermoelectric properties of Mg2(Si, Sn) solid solutions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3

Citation Types

0
3
0

Year Published

2024
2024
2024
2024

Publication Types

Select...
3

Relationship

0
3

Authors

Journals

citations
Cited by 3 publications
(3 citation statements)
references
References 57 publications
0
3
0
Order By: Relevance
“…The flaws limiting strength include volume type (e.g., pores/cavities, agglomerates, porous regions, inclusions, and large grains), surface type (e.g., handling damage, machining damage, pitting, oxidation, and chemical product), and edge type (e.g., edge chipping) . As shown in Figure b, the Mg-deficient compound Mg 1.9 (SiSn) sintered at 973 K for 4 h in a vacuum after mechanical alloying had different defects like elemental agglomeration (Si), pores, etc . These defects lead to unpredictable changes or degradation in TE performance.…”
Section: Challenges and Major Issues Of The Magnesium-based Te Materi...mentioning
confidence: 99%
See 2 more Smart Citations
“…The flaws limiting strength include volume type (e.g., pores/cavities, agglomerates, porous regions, inclusions, and large grains), surface type (e.g., handling damage, machining damage, pitting, oxidation, and chemical product), and edge type (e.g., edge chipping) . As shown in Figure b, the Mg-deficient compound Mg 1.9 (SiSn) sintered at 973 K for 4 h in a vacuum after mechanical alloying had different defects like elemental agglomeration (Si), pores, etc . These defects lead to unpredictable changes or degradation in TE performance.…”
Section: Challenges and Major Issues Of The Magnesium-based Te Materi...mentioning
confidence: 99%
“… 69 As shown in Figure 3 b, the Mg-deficient compound Mg 1.9 (SiSn) sintered at 973 K for 4 h in a vacuum after mechanical alloying had different defects like elemental agglomeration (Si), pores, etc. 70 These defects lead to unpredictable changes or degradation in TE performance. Meanwhile, suitable mechanical strength and hardness are crucial to prevent surface damage during handling, and leg production such as the cutting and packing process.…”
Section: Challenges and Major Issues Of The Magnesium-based Te Materi...mentioning
confidence: 99%