Effect of the addition of room temperature ionic liquid and ZnO nanoparticles on the wear and scratch resistance of epoxy resin

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
5

Citation Types

1
64
0
4

Year Published

2010
2010
2021
2021

Publication Types

Select...
8
1

Relationship

2
7

Authors

Journals

citations
Cited by 109 publications
(69 citation statements)
references
References 27 publications
1
64
0
4
Order By: Relevance
“…Ionic liquids (ILs) have been applied as sole crosslinkers for epoxy resin [1][2][3][4][5] or admixtures for epoxy systems cured with conventional hardeners that allowed to modify the properties of the final epoxy materials [3,[6][7][8]. ILs have been used together with polyamine or anhydride hardeners in order to modify epoxy curing process as well as materials glass transition temperature [7,8], lubrication [6], or to improve (nano)filler dispersion [9][10][11].…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…Ionic liquids (ILs) have been applied as sole crosslinkers for epoxy resin [1][2][3][4][5] or admixtures for epoxy systems cured with conventional hardeners that allowed to modify the properties of the final epoxy materials [3,[6][7][8]. ILs have been used together with polyamine or anhydride hardeners in order to modify epoxy curing process as well as materials glass transition temperature [7,8], lubrication [6], or to improve (nano)filler dispersion [9][10][11].…”
Section: Introductionmentioning
confidence: 99%
“…ILs have been used together with polyamine or anhydride hardeners in order to modify epoxy curing process as well as materials glass transition temperature [7,8], lubrication [6], or to improve (nano)filler dispersion [9][10][11]. The epoxy compositions with the most often used 1-alkyl-3-methylimidazolium ILs exhibited pot life at ambient temperature: 50-60 days where counteranions were chloride or tetrafluoroborate (3 wt parts/ 100 wt parts of epoxy resin, 3 phr) [4,12].…”
Section: Introductionmentioning
confidence: 99%
“…[16,17] This modified epoxy system presents antistatic properties, heat, abrasion, and water resistances as well as mechanical strength and transparency. [17] Sanes et al [18,19] reported the addition of imidazolium-based IL salts in epoxy systems cured with room temperature hardener to plasticize the epoxy network and reduce the friction coefficient and wear rate of the final material.…”
Section: Introductionmentioning
confidence: 99%
“…In recent studies, we have shown that it is possible to improve the tribological performance of thermoplastics [34][35][36][37][38][39] and of epoxy resin [40] against steel by preparing new dispersions containing variable concentrations of ILs or IL-modified ZnO nanoparticles.…”
Section: Introductionmentioning
confidence: 99%