Abstract: Glass fiber reinforced polymers GFRPs are increasingly being applied as structural materials with their advantages of light weight and high strength in the fields of aerospace engineering and rapid transport engineering. To strengthen the GFRPs, sheet electron beam (EB) irradiation under low potential has been performed homogeneously. Effects of EB-irradiation on Charpy impact value of GFRPs have been studied. The irradiation, applied as a short-time treatment at room temperature, enhances the impact value of … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
22
0

Year Published

2008
2008
2021
2021

Publication Types

Select...
8

Relationship

5
3

Authors

Journals

citations
Cited by 40 publications
(22 citation statements)
references
References 13 publications
0
22
0
Order By: Relevance
“…12,2631) Accumulative probabilities (P: P i , P max , P B , P S¾ , P Sf ) are initial stiffness ((d¸/d¾) i ), maximum stiffness ((d¸/d¾) max ), tensile shear strength (¸B), its strain (¾ B ) and fracture strain (¾ Sf ), which are employed here to quantitatively analyze our experimental values by the following equation:…”
Section: Tensile Shear Strength Its Strain and Fracture Strainmentioning
confidence: 99%
“…12,2631) Accumulative probabilities (P: P i , P max , P B , P S¾ , P Sf ) are initial stiffness ((d¸/d¾) i ), maximum stiffness ((d¸/d¾) max ), tensile shear strength (¸B), its strain (¾ B ) and fracture strain (¾ Sf ), which are employed here to quantitatively analyze our experimental values by the following equation:…”
Section: Tensile Shear Strength Its Strain and Fracture Strainmentioning
confidence: 99%
“…1 and Fig. 4, external [5][6][7][8][10][11][12][13][14][15][16] and internal 9) HLEBI activation fabrication processes of [PP] 6 [GF-CSM] 5 CSM-CFRTP are different. Since strengthening GFRP bulk has been suggested and developed to reinforce the GF/PP interface adhesion by the internal HLEBI activation of GFs prior to dipping in the PP (see broken lines in Fig.…”
Section: Hlebi-strengthening Gfrp Surface Comparedmentioning
confidence: 99%
“…Therefore, although internal activation has its suitable applications, to be cost and time effective we propose the conventional simpler process [10][11][12][13][14][15][16] 5 CSM-GFRTP will increase Charpy impact strength signi cantly over the untreated especially at low P f < 0.10 while increasing statistical reliability about as much as that of the internal HLEBI activation. When applying to actual parts, careful consideration to adjusting HLEBI to get optimum dose is highly recommended for reliability and safety.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…11,12) These effects are mainly caused by surface energy induced by the irradiation with the formation of active terminated atoms with dangling bonds. When HLEBI improves the joining between different polymers and metals/polymers, 13,14) rapid and safety adhesion between different polymers by using HLEBI has been successfully developed.…”
Section: Introductionmentioning
confidence: 99%