2012
DOI: 10.1179/174591911x13167804920948
|View full text |Cite
|
Sign up to set email alerts
|

Effects of NO3in NaCl solution on corrosion protection of AZ91D magnesium alloy coated with silane films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

0
7
0

Year Published

2014
2014
2022
2022

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 12 publications
(7 citation statements)
references
References 39 publications
0
7
0
Order By: Relevance
“…It is worth mentioning here that, despite a few reports on the remarkable inhibition effects of NO 3 − on the corrosion of magnesium and its alloys [ 10 , 28 , 29 , 30 ], the inhibition mechanism has not been addressed in detail.…”
Section: Inorganic Inhibitorsmentioning
confidence: 99%
See 2 more Smart Citations
“…It is worth mentioning here that, despite a few reports on the remarkable inhibition effects of NO 3 − on the corrosion of magnesium and its alloys [ 10 , 28 , 29 , 30 ], the inhibition mechanism has not been addressed in detail.…”
Section: Inorganic Inhibitorsmentioning
confidence: 99%
“…Nitrates are commonly used as corrosion inhibitors for steel. A few reports also showed their significant positive effect on magnesium alloys [ 10 , 28 , 29 , 30 , 69 ]. A universal high inhibition effect of KNO 3 has been observed by Lamaka et al [ 10 ].…”
Section: Inorganic Inhibitorsmentioning
confidence: 99%
See 1 more Smart Citation
“…Several coating techniques have been adopted to improve the corrosion resistance of magnesium alloys. These include electrodeposition or electroless plating , plasma electrolytic oxidation , chemical conversion , anodizing , and sol–gel process etc., each has their own advantages and disadvantages.…”
Section: Introductionmentioning
confidence: 99%
“…Interestingly, the nitrate ion was reported to be an efficient corrosion inhibitor 21,26 and a favorable electrolyte for Mg−air batteries. 11,15 Clearly, in this work, when the harsher environment is used, nitrate reduced the utilization efficiency of the Mg anode at the applied discharge current density of 5 mA/cm 2 and caused nonuniform dissolution with a visible layer of corrosion products accumulated over the surface (Figure 2(e,f)).…”
mentioning
confidence: 99%