Abstract:The major factors and affection for hydrothermal synthesis of ammonium vanadate in microwave irradiation was investigated and optimized. The obtained material was a pure (NH 4 ) 2 V 6 O 16 phase with regular spindle and rhombic crystal shapes. Transmission electron microscope and selected-area electron diffraction patterns confirmed that the microwave irradiation-assisted hydrothermal treatments altered the growth pattern and expanded the [-1 0 0] interplanar spacing by approximately ß8%-12% compared to the st… Show more
“…While exceeded 30 min, as water evaporates, other impurity ions such as SO 4 2− and Na + were crystallized and mixed with the vanadium precipitation product. 40 The precursor has low purity, resulted a low N content in vanadium nitride. As shown in Fig.…”
Section: Resultsmentioning
confidence: 99%
“…As the temperature is increased, the water evaporates and a large number of voids appear in the precursor, with a narrow contact area with N 2 and a lack of Table 2 Thermodynamics analysis data of calcination deamination process and Na + were crystallized and mixed with the vanadium precipitation product. 40 The precursor has low purity, resulted a low N content in vanadium nitride. As shown in Fig.…”
The particle size of the precursor is reduced, while it is easier for N2 to enter the material. A new porous structure appeared and the specific surface area increased, which increases the reaction interface.
“…While exceeded 30 min, as water evaporates, other impurity ions such as SO 4 2− and Na + were crystallized and mixed with the vanadium precipitation product. 40 The precursor has low purity, resulted a low N content in vanadium nitride. As shown in Fig.…”
Section: Resultsmentioning
confidence: 99%
“…As the temperature is increased, the water evaporates and a large number of voids appear in the precursor, with a narrow contact area with N 2 and a lack of Table 2 Thermodynamics analysis data of calcination deamination process and Na + were crystallized and mixed with the vanadium precipitation product. 40 The precursor has low purity, resulted a low N content in vanadium nitride. As shown in Fig.…”
The particle size of the precursor is reduced, while it is easier for N2 to enter the material. A new porous structure appeared and the specific surface area increased, which increases the reaction interface.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.