2011
DOI: 10.1016/j.jallcom.2011.06.107
|View full text |Cite
|
Sign up to set email alerts
|

Electrocatalytic behaviour of NiBi coatings for hydrogen evolution reaction in alkaline medium

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
12
0

Year Published

2013
2013
2022
2022

Publication Types

Select...
8

Relationship

1
7

Authors

Journals

citations
Cited by 27 publications
(12 citation statements)
references
References 57 publications
0
12
0
Order By: Relevance
“…The oldest process for hydrogen production is the process of water electrolysis where the most important component of the system is the type of a chosen material for the electrodes design. Nickel (Ni) is a frequently used material in hydrogen generation process because of its good properties both as the catalyst and the electrode [11][12][13][14][15]. It is founding in forms of a bulk, the foam, a raney, a mesh and different alloys.…”
Section: Introductionmentioning
confidence: 99%
“…The oldest process for hydrogen production is the process of water electrolysis where the most important component of the system is the type of a chosen material for the electrodes design. Nickel (Ni) is a frequently used material in hydrogen generation process because of its good properties both as the catalyst and the electrode [11][12][13][14][15]. It is founding in forms of a bulk, the foam, a raney, a mesh and different alloys.…”
Section: Introductionmentioning
confidence: 99%
“…During forward scan, the appearance of the anodic peak at −0.6 V indicates Ni/Ni 2+ oxidation, followed by the change of Ni(OH) 2 to Ni(OH) 2 until 0.4 V (vs Ag/AgCl). Ni 2+ /Ni 3+ oxidation is detected at 0.45 V, whereas the Ni 3+ /Ni 2+ is seen at roughly 0.35 V as cathodic peak in backward scan 45‐48 . The anodic current increase at −0.25 V is corresponding to the transformation of Co/Co 2+ oxidation 1,49‐51 .…”
Section: Resultsmentioning
confidence: 92%
“…Ni 2+ /Ni 3+ oxidation is detected at 0.45 V, whereas the Ni 3+ /Ni 2+ is seen at roughly 0.35 V as cathodic peak in backward scan. [45][46][47][48] The anodic current increase at À0.25 V is corresponding to the transformation of Co/Co 2+ oxidation. 1,[49][50][51] In the voltammogram of…”
Section: Production Of Electrocatalysts and Investigation Of Hpementioning
confidence: 99%
“…In this work, ternary coating was favored on graphite and Ni-Co-Cu was employed, based on the outstanding performance of binary coatings combining Ni-Co and Ni-Cu in the literature (Solmaz et al, 2008;Solmaz et al, 2009;Demirdelen et al, 2020). Considering the literature, the coating's Co and Cu mole ratios should be kept low in comparison to the Ni mole ratio (Mert and Kardaş, 2011;Sun et al, 2021). The electrodeposition of nickel, cobalt and copper was performed by galvanostatically using Iviumstat Electrochemical Interface with a three-electrode configuration.…”
Section: Methodsmentioning