Electroplated CoNiMnP-based permanent magnetic films with thickness of 4 m, 25 m and 43.5 m were fabricated and tested. Composed of 76.38 wt% Co, 16.66 wt% Ni, 3.64 wt% P and 2.32 wt% Mn, the films exhibited good surface morphology. In the case of 4 m thick film, we successfully achieved a high lateral coercivity of 711Oe, a retentivity up to 8933Gs and an energy density of 16.9kJ/m 3 . The film thickness dependence of magnetic property was also investigated, showing a decrease of the retentivity and coercivity with the increase in thickness. In addition, it was observed that Zn as an additive could improve the surface morphology by eliminating micro cracks.