Electroplating and Surface Analysis

Abstract: The interest in scientific research within the metal finishing sector is growing. The demand for durable metals and adaptable manufacturing processes are increasing across a wide range of applications, from aerospace and automotive to machinery and jewelry. An essential step in the production line is the surface engineering of metals, as this determines the final appearance and functionality of a product. Therein electroplating is recognized as a mature technology allowing the low cost fabrication of defined s… Show more